The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 31, 2023

Filed:

Oct. 06, 2021
Applicant:

3m Innovative Properties Company, St. Paul, MN (US);

Inventors:

Jing Fang, Shanghai, CN;

Dong Yang, Shanghai, CN;

Jeffrey W. McCutcheon, Baldwin, WI (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01B 1/22 (2006.01); C09J 9/02 (2006.01); C09J 201/02 (2006.01);
U.S. Cl.
CPC ...
C09J 9/02 (2013.01); C09J 201/02 (2013.01); H01B 1/22 (2013.01); C09J 2301/302 (2020.08); C09J 2301/312 (2020.08); C09J 2301/314 (2020.08);
Abstract

An electrically conductive adhesive layer includes an adhesive material; a plurality of electrically conductive dendritic first particles dispersed in the adhesive material and having a cumulative 50% particle diameter D50 in a range from about 20 micrometers to about 40 micrometers; and a plurality of electrically conductive substantially planar second particles dispersed in the adhesive material and having a cumulative 50% particle diameter D50 in a range from about 40 micrometers to about 70 micrometers. The adhesive layer has an average thickness in a range from about 15 micrometers to about 35 micrometers, an electrical resistance in a thickness direction of less than about 30 milliohms, and a peel strength of at least 0.1 N/mm from a stainless steel surface after a dwell time of about 20 minutes at 22° C.