The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 24, 2023

Filed:

Oct. 24, 2019
Applicant:

Nippon Steel Corporation, Tokyo, JP;

Inventors:

Hiroshi Fujimura, Tokyo, JP;

Satoshi Kano, Tokyo, JP;

Miho Tomita, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/12 (2006.01); C22C 38/02 (2006.01); C22C 38/00 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C21D 8/02 (2006.01); C21D 9/00 (2006.01); C21D 9/46 (2006.01); H01F 1/147 (2006.01); B21D 28/02 (2006.01);
U.S. Cl.
CPC ...
C21D 8/12 (2013.01); B21D 28/02 (2013.01); C21D 8/0263 (2013.01); C21D 9/0012 (2013.01); C21D 9/46 (2013.01); C22C 38/004 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); H01F 1/14775 (2013.01); C21D 2261/00 (2013.01); C22C 2202/02 (2013.01);
Abstract

Provided are a non-oriented electrical steel sheet with which it is possible to improve steel sheet transferability even when punching is performed successively at high speed, and a method of manufacturing a stacked core using the same. The non-oriented electrical steel sheet contains, by mass percent, Si: 2.0 to 5.0%, Mn: 0.4 to 5.0%, Al≤3.0%, C: 0.0008 to 0.0100%, N≤0.0030%, S≤0.0030%, and Ti≤0.0060%, wherein the product of the contents of Mn and C is 0.004 to 0.05 mass %, the yield strength in rolling direction is more than or equal to 600 MPa, and the Young's modulus is more than or equal to 200 GPa. In the method of manufacturing a stacked core, when manufacturing a stacked core using a progressive die, the steel sheet transfer speed V (m/s) satisfies expression (1). V: Vto V(1) V=( 1/25)√(t×E×YS) (2) V=( 1/25)√(t×120000) (3) t: Steel sheet thickness (mm), E: Young's ratio (GPa), YS: Yield strength (MPa).