The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 17, 2023

Filed:

Nov. 22, 2022
Applicant:

W. L. Gore & Associates Gmbh, Putzbrunn, DE;

Inventors:

Andrea Doernhoefer, Hoehenkirchen, DE;

Michael Rittmann, Putzbrunn, DE;

Klaus Seibert, Emmersdingen, DE;

Alexander Zaggl, Aying, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 27/32 (2006.01); B32B 5/16 (2006.01); B32B 15/06 (2006.01); B32B 15/20 (2006.01); B32B 25/08 (2006.01); B32B 25/12 (2006.01); B32B 25/18 (2006.01); B32B 25/20 (2006.01); B32B 27/40 (2006.01);
U.S. Cl.
CPC ...
B32B 27/322 (2013.01); B32B 5/16 (2013.01); B32B 15/06 (2013.01); B32B 15/20 (2013.01); B32B 25/08 (2013.01); B32B 25/12 (2013.01); B32B 25/18 (2013.01); B32B 25/20 (2013.01); B32B 27/40 (2013.01); B32B 2250/03 (2013.01); B32B 2264/105 (2013.01); B32B 2264/108 (2013.01); B32B 2307/202 (2013.01); B32B 2307/204 (2013.01); B32B 2307/732 (2013.01); B32B 2457/00 (2013.01);
Abstract

The present disclosure is directed to dielectric elastomeric composites that include a retainable processing membrane, an elastomer material, and an electrically conductive material. The elastomer layer may be partially imbibed into the retainable processing membrane. The retainable processing membrane may be porous. The retainable processing membrane is compacted in the transverse direction, machine direction, or in both directions prior to the application of an elastomer material and an electrically conductive material. The compaction of the retainable processing membrane may form structured folds or folded fibrils in the membrane, giving the retainable processing membrane a low modulus and flexibility. In some embodiments, the dielectric composites are positioned in a stacked configuration. Alternatively, the dielectric elastomeric composites may have a wound configuration. The dielectric composites have a total thickness less than about 170 μm. The dielectric elastomeric composites may be used, for example, in dielectric elastomer actuators, sensors, and in energy harvesting.