The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 10, 2023

Filed:

Jul. 31, 2018
Applicant:

Sumitomo Metal Mining Co., Ltd., Tokyo, JP;

Inventors:

Hiroko Oshita, Niihama, JP;

Kazuomi Ryoshi, Niihama, JP;

Taira Aida, Niihama, JP;

Koji Yamaji, Niihama, JP;

Jiro Okada, Niihama, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); H01M 4/505 (2010.01); H01M 10/0525 (2010.01); H01M 4/04 (2006.01); H01M 4/131 (2010.01); H01M 4/1391 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); H01M 4/0404 (2013.01); H01M 4/0471 (2013.01); H01M 4/131 (2013.01); H01M 4/1391 (2013.01); H01M 4/505 (2013.01); H01M 10/0525 (2013.01); H01M 2004/028 (2013.01); Y02E 60/10 (2013.01);
Abstract

The present invention provides a lithium-nickel-manganese-cobalt composite oxide in which the reactivity between a lithium raw material and a metal composite hydroxide is improved so that a high low-temperature output characteristic can be achieved, a method for manufacturing the composite oxide, and a positive electrode active material and the like without causing a problem of gelation during the paste preparation. A positive electrode active material for non-aqueous electrolyte secondary batteries, including a lithium-metal composite oxide powder including a secondary particle configured by aggregating primary particles containing lithium, nickel, manganese, and cobalt, or a lithium-metal composite oxide powder including both the primary particles and the secondary particle. The secondary particle has a solid structure inside as a main inside structure, the slurry pH is 11.5 or less, the soluble lithium content rate is 0.5 [% by mass] or less, and the specific surface area is 1.0 to 2.0 [m/g].