The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 10, 2023

Filed:

Feb. 21, 2019
Applicant:

Asahi Kasei Kabushiki Kaisha, Tokyo, JP;

Inventors:

Kazuya Iseda, Tokyo, JP;

Kentaro Shiraishi, Tokyo, JP;

Mifuyu Niwa, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/04 (2006.01); B32B 17/06 (2006.01); C09D 175/04 (2006.01); C09D 7/61 (2018.01); C09D 7/47 (2018.01); C03C 17/00 (2006.01); C03C 17/30 (2006.01); C09D 5/02 (2006.01); B32B 17/10 (2006.01);
U.S. Cl.
CPC ...
C09D 175/04 (2013.01); B32B 17/10 (2013.01); C03C 17/009 (2013.01); C03C 17/30 (2013.01); C09D 5/024 (2013.01); C09D 7/47 (2018.01); C09D 7/61 (2018.01); C03C 2217/75 (2013.01);
Abstract

The problem addressed by the present invention is to provide an antifogging coating film having excellent antifogging property, antifogging persistence, persistence of appearance, and elution resistance. The coating film according to the present invention contains a metal oxide (A) and a hydrophilic compound (B); the height of the eluate by a coating film surface elution test is 1.0 μm or less; this test is carried out by placing 10 μL of deionized water on the coating film, allowing the film to stand for 24 hours in a 23° C., 50% RH environment, measuring the eluate height of 20 locations selected randomly within a 10 cmrange on the coating film surface, and determining the maximum height; and the water contact angle measured after subjecting the coating film to a moisture resistance test by exposure for 24 hours in an 85° C., 85% RH environment followed by standing for one hour in a 23° C., 50% RH environment, is less than 40°. Preferably, the elution level per coating film unit volume by a coating film total elution test is 40 mg/cmor less, and this test is carried out by immersing the coating film in 23° C. deionized water for 24 hours, then measuring the weight of the coating film eluate recovered from the deionized water.