The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 10, 2023

Filed:

Oct. 04, 2019
Applicant:

Bridgestone Corporation, Tokyo, JP;

Inventors:

Kenji Nakatani, Tokyo, JP;

Kentaro Kumaki, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 9/06 (2006.01); C08L 7/00 (2006.01); C08L 15/00 (2006.01); B60C 1/00 (2006.01); C08C 19/25 (2006.01); C08F 136/06 (2006.01); C08F 136/08 (2006.01); C08K 3/04 (2006.01); C08K 3/36 (2006.01);
U.S. Cl.
CPC ...
C08L 9/06 (2013.01); B60C 1/0016 (2013.01); C08C 19/25 (2013.01); C08F 136/06 (2013.01); C08F 136/08 (2013.01); C08K 3/04 (2013.01); C08K 3/36 (2013.01); C08L 7/00 (2013.01); C08L 15/00 (2013.01); C08L 2205/025 (2013.01); C08L 2205/035 (2013.01); C08L 2205/08 (2013.01);
Abstract

To provide a rubber composition in which wet performance, wear resistance, low rolling resistance, and breaking resistance are highly balanced. A rubber composition comprising a rubber component comprising at least three polymers and a filler, wherein the rubber component is separated into at least two polymer phases: a polymer phase (1) with the highest tan δ peak temperature; and a polymer phase (2) with the lowest peak temperature; the polymer phases (1) and (2) are incompatible with each other; the polymer phase (1) at least comprises the modified conjugated diene-based polymers (A1) and (A2), and the filler; the modified conjugated diene-based polymer (A1) has a particular weight-average molecular weight and a particular contracting factor (g'); and when a filler concentration and an average aggregate area of the filler in the polymer phase (1) are defined as X and Y, respectively, an formula (1): Y<4.8X+1200 is satisfied.