The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 10, 2023

Filed:

Dec. 10, 2019
Applicant:

Ifp Energies Nouvelles, Rueil-Malmaison, FR;

Inventor:

Elodie Devers, Rueil-Malmaison, FR;

Assignee:

IFP Energies nouvelles, Rueil-Malmaison, FR;

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B01J 27/28 (2006.01); B01J 21/04 (2006.01); B01J 27/19 (2006.01); B01J 38/02 (2006.01); B01J 38/12 (2006.01); B01J 38/62 (2006.01); C10G 45/08 (2006.01); C10G 47/12 (2006.01);
U.S. Cl.
CPC ...
B01J 27/285 (2013.01); B01J 21/04 (2013.01); B01J 27/19 (2013.01); B01J 38/02 (2013.01); B01J 38/12 (2013.01); B01J 38/62 (2013.01); C10G 45/08 (2013.01); C10G 47/12 (2013.01); C10G 2300/1059 (2013.01); C10G 2300/202 (2013.01); C10G 2300/706 (2013.01); C10G 2400/02 (2013.01);
Abstract

The invention concerns a method for rejuvenating an at least partially used catalyst originating from a hydroprocessing and/or hydrocracking process, the at least partially used catalyst being derived from a fresh catalyst comprising at least one group VIII metal (in particular, Co), at least one group VIB metal (in particular, Mo), an oxide support, and optionally phosphorus, the method comprising the steps: ⋅a) regenerating the at least partially used catalyst in a gas stream containing oxygen at a temperature between 300° C. and 550° C. so as to obtain a regenerated catalyst, ⋅b) then placing the regenerated catalyst in contact with phosphoric acid and an organic acid, each having acidity constant pKa greater than 1.5, ⋅c) performing a drying step at a temperature less than 200° C. without subsequently calcining it, so as to obtain a rejuvenated catalyst.