The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 03, 2023

Filed:

Jan. 30, 2020
Applicant:

Benteler Automobiltechnik Gmbh, Paderborn, DE;

Inventors:

Jochem Grewe, Salzkotten, DE;

Feng Jiao, Paderborn, DE;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22F 1/05 (2006.01); B21D 22/02 (2006.01); C21D 9/46 (2006.01); C22C 21/08 (2006.01); C22C 21/14 (2006.01); C22C 21/16 (2006.01); C22C 21/02 (2006.01); B21D 53/88 (2006.01); B21D 53/74 (2006.01);
U.S. Cl.
CPC ...
C22F 1/05 (2013.01); B21D 22/02 (2013.01); C21D 9/46 (2013.01); C22C 21/02 (2013.01); C22C 21/08 (2013.01); C22C 21/14 (2013.01); C22C 21/16 (2013.01); B21D 53/74 (2013.01); B21D 53/88 (2013.01);
Abstract

The present disclosure relates to a method for producing a motor vehicle component from a 6000-series aluminum alloy having the following method steps: providing a blank made of a 6000-series aluminum alloy, rapid heating of the blank by means of contact plates to a temperature between 450° C. and 600° C. in a time less than 20 seconds, ending of the heating procedure and optional homogenizing when a grain size between 20 and 50 μm has resulted, quenching the blank thus tempered to a temperature less than or equal to 100° C., in a time less than 20 seconds, wherein the rapid heating and quenching of the blank is carried out in a total time of less than 50 seconds, applying a lubricant, at 20° C. to 100° C., forming the cooled blank in a forming tool, wherein the time between beginning the rapid heating and beginning the forming is less than 45 seconds, aging.