The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 26, 2023

Filed:

Mar. 08, 2017
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Takeshi Omura, Tokyo, JP;

Hirotaka Inoue, Tokyo, JP;

Shigehiro Takajo, Tokyo, JP;

Seiji Okabe, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/12 (2006.01); H01F 1/147 (2006.01); C22C 38/60 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/34 (2006.01);
U.S. Cl.
CPC ...
C21D 8/1277 (2013.01); C21D 8/12 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); H01F 1/147 (2013.01); C21D 2201/05 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/34 (2013.01); C22C 38/60 (2013.01);
Abstract

To reduce variations in iron loss among materials subjected to magnetic domain refining by electron beam irradiation and to stably obtain good iron loss properties, disclosed is a method of producing a grain-oriented electrical steel sheet including performing magnetic domain refining treatment by irradiating with an electron beam, in a pressure reduced area, a surface of a grain-oriented electrical steel sheet after subjection to final annealing, the method further including: before the irradiating with the electron beam, delivering the grain-oriented electrical steel sheet wound in a coil shape and heating the delivered grain-oriented electrical steel sheet to 50° C. or higher; and then cooling the grain-oriented electrical steel sheet such that the grain-oriented electrical steel sheet has a temperature of lower than 50° C. at the time of entering the pressure reduced area.