The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 12, 2023

Filed:

Sep. 16, 2022
Applicant:

Stmicroelectronics S.r.l., Agrate Brianza, IT;

Inventors:

Michele Calabretta, Giarre, IT;

Crocifisso Marco Antonio Renna, Floridia, IT;

Sebastiano Russo, Santa Tecla di Acireale, IT;

Marco Alfio Torrisi, Aci Sant'Antonio, IT;

Assignee:

STMICROELECTRONICS S.R.L., Agrate Brianza, IT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01L 23/00 (2006.01); B23K 35/26 (2006.01); C22C 13/00 (2006.01); H01L 23/31 (2006.01); H01L 23/495 (2006.01); B23K 101/40 (2006.01);
U.S. Cl.
CPC ...
H01L 24/29 (2013.01); B23K 35/262 (2013.01); C22C 13/00 (2013.01); H01L 23/3121 (2013.01); H01L 23/49513 (2013.01); H01L 23/49541 (2013.01); H01L 23/49579 (2013.01); H01L 24/27 (2013.01); H01L 24/32 (2013.01); H01L 24/83 (2013.01); B23K 2101/40 (2018.08); H01L 24/48 (2013.01); H01L 24/73 (2013.01); H01L 2224/2912 (2013.01); H01L 2224/29105 (2013.01); H01L 2224/29109 (2013.01); H01L 2224/29111 (2013.01); H01L 2224/29139 (2013.01); H01L 2224/29147 (2013.01); H01L 2224/29155 (2013.01); H01L 2224/32245 (2013.01); H01L 2224/48091 (2013.01); H01L 2224/48245 (2013.01); H01L 2224/73265 (2013.01); H01L 2224/83192 (2013.01); H01L 2224/83801 (2013.01); H01L 2924/014 (2013.01); H01L 2924/20109 (2013.01);
Abstract

A method for soldering a die obtained using the semiconductor technique with a leadframe, comprising the steps of providing a leadframe, which has at least one surface made at least partially of copper; providing a die, which has at least one surface coated with a metal layer; applying to the surface a solder alloy comprising at least 40 wt % of tin or at least 50% of indium or at least 50% of gallium, without lead, and heating the alloy to a temperature of at least 380° C. to form a drop of solder alloy; providing a die, which has at least one surface coated with a metal layer; and setting the metal layer in contact with the drop of solder alloy to form the soldered connection with the leadframe. Moreover, a device obtained with said method is provided.