The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 12, 2023

Filed:

Sep. 08, 2017
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Souichiro Yoshizaki, Tokyo, JP;

Makoto Watanabe, Tokyo, JP;

Ryuichi Suehiro, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01F 1/18 (2006.01); C21D 8/12 (2006.01); C22C 38/00 (2006.01); C23C 22/12 (2006.01); C23C 22/18 (2006.01); C23C 22/20 (2006.01); C23C 22/22 (2006.01); C23C 22/74 (2006.01); H01F 1/147 (2006.01);
U.S. Cl.
CPC ...
H01F 1/18 (2013.01); C21D 8/1283 (2013.01); C21D 8/1288 (2013.01); C22C 38/00 (2013.01); C23C 22/12 (2013.01); C23C 22/188 (2013.01); C23C 22/20 (2013.01); C23C 22/22 (2013.01); C23C 22/74 (2013.01); H01F 1/147 (2013.01); C21D 2201/05 (2013.01);
Abstract

A grain-oriented magnetic steel sheet with chromium-free insulating tension coating includes a grain-oriented magnetic steel sheet and an insulating tension coating containing a phosphate salt and silica on a surface of the grain-oriented magnetic steel sheet, the coating further including a crystalline compound represented by the general formula (1): MM(XO). . . (1). A method for producing a grain-oriented magnetic steel sheet with chromium-free insulating tension coating includes applying an insulating tension coating liquid to a surface of a finish annealed grain-oriented magnetic steel sheet, the coating liquid including colloidal silica, a phosphate salt and a metal element M-containing compound in a specific ratio, and heat treating the steel sheet at least one time at a temperature of not less than 900° C. in an atmosphere including a non-oxidizing gas and having a dew point of not more than 0° C.