The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 08, 2023

Filed:

May. 28, 2020
Applicant:

Furukawa Electric Co., Ltd., Tokyo, JP;

Inventors:

Hiroki Chiba, Tokyo, JP;

Masaki Nishiguchi, Tokyo, JP;

Arifumi Matsumura, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08L 27/16 (2006.01); C08K 3/22 (2006.01); C08K 3/26 (2006.01); C08K 3/36 (2006.01); C08K 5/14 (2006.01); C08L 23/26 (2006.01); C08L 27/18 (2006.01); C08L 51/04 (2006.01);
U.S. Cl.
CPC ...
C08L 27/16 (2013.01); C08K 3/22 (2013.01); C08K 3/26 (2013.01); C08K 3/36 (2013.01); C08K 5/14 (2013.01); C08L 23/26 (2013.01); C08L 27/18 (2013.01); C08L 51/04 (2013.01); C08K 2003/2296 (2013.01); C08K 2003/265 (2013.01); C08L 2201/08 (2013.01); C08L 2203/206 (2013.01); C08L 2310/00 (2013.01); C08L 2312/08 (2013.01);
Abstract

A method of producing a heat-resistant crosslinked fluororubber formed body, including: step (1) melt-mixing, with respect to 100 mass parts of base rubber containing 60 to 99 mass % of fluororubber and 1 to 40 mass % of ethylene-based copolymer resin modified with unsaturated carboxylic acid, 0.003 to 0.5 mass parts of organic peroxide, 0.5 to 400 mass parts of inorganic filler, 2 to 15 mass parts of silane coupling agent, and silanol condensation catalyst, in which the step (1) includes, step (a) melt-mixing all or part of the base rubber, the organic peroxide, the inorganic filler and the silane coupling agent at a temperature equal to or higher than a decomposition temperature of the organic peroxide, and step (b) melt-mixing a remainder of the base rubber, and the silanol condensation catalyst, to melt-mix the thus-modified ethylene-based copolymer resin in at least one of the steps (a) and (b).