The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 11, 2023

Filed:

Mar. 08, 2022
Applicant:

Venator Germany Gmbh, Duisburg, DE;

Inventors:

Juergen Philipp Kastner, Essen, DE;

Uwe Rosin, Kamp-Lintfort, DE;

Assignee:

VENATOR GERMANY GMBH, Duisburg, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C01G 23/08 (2006.01); C01G 23/053 (2006.01); C09C 1/36 (2006.01); C01G 23/047 (2006.01);
U.S. Cl.
CPC ...
C01G 23/08 (2013.01); C01G 23/047 (2013.01); C01G 23/0532 (2013.01); C09C 1/3669 (2013.01); C09C 1/3676 (2013.01); C09C 1/3684 (2013.01); C01P 2002/60 (2013.01); C01P 2004/62 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); C01P 2006/14 (2013.01); C01P 2006/64 (2013.01); C01P 2006/80 (2013.01);
Abstract

A process for producing a particulate TiOincludes supplementing metatitanic acid with an alkali compound in a quantity of 1200 ppm to 2400 ppm of alkali, with a phosphorus compound in a quantity of 0.1 wt.-% to 0.3 wt.-% by weight of P, expressed as phosphorus, and with an aluminum compound in a quantity of 1 ppm to 1000 ppm of Al, expressed as Al, to obtain a mixture. The quantity of the alkali compound, of the phosphorus compound, and of the aluminum compound are with respect to the TiOcontent. The mixture is calcined at a constant temperature of 940° C. to 1020° C. until a numerical fraction Xof TiOhas a primary crystallite size of at least 200 nm, to obtain a calcined mixture. The calcined mixture is cooled to obtain a cooled calcined mixture. The cooled calcined mixture is grinded to obtain the particulate TiO.