The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 04, 2023

Filed:

Nov. 15, 2019
Applicant:

Mucell Extrusion, Llc, Woburn, MA (US);

Inventors:

Mehdi Saniei, Belmont, MA (US);

James K. Sakorafos, Shrewsbury, MA (US);

Nicholas R. Torraco, Arlington, MA (US);

Mark E. Lindenfelzer, Milton, MA (US);

Assignee:

MuCell Extrusion, LLC, Woburn, MA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 27/08 (2006.01); B29C 48/00 (2019.01); B29C 48/18 (2019.01); B32B 27/06 (2006.01); B32B 27/32 (2006.01); B29K 23/00 (2006.01);
U.S. Cl.
CPC ...
B32B 27/08 (2013.01); B29C 48/022 (2019.02); B29C 48/18 (2019.02); B32B 27/065 (2013.01); B32B 27/32 (2013.01); B29K 2023/06 (2013.01); B29K 2023/18 (2013.01); B32B 2323/043 (2013.01); B32B 2323/046 (2013.01);
Abstract

This invention relates to an anisotropic multilayer film and the process of making a multilayer film, wherein a supercritical blowing agent is introduced to at least one layer, wherein at least one layer comprises 10 to 100 percent by weight LLDPE with a melt index of 0.2 to 2 g/10 min. The film in this invention can have a surface with an average Sheffield smoothness, according to TAPPI T 538, of less than 100. The film in this invention can have a puncture propagation tear resistance, in accordance with ASTM D2582, greater than 500 g/mil.