The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 13, 2023

Filed:

Jan. 22, 2018
Applicant:

Hyundai Steel Company, Incheon, KR;

Inventors:

Jun Ho Chung, Gyeonggi-do, KR;

Tae Hyung Kim, Gyeonggi-do, KR;

Ju Sang Lee, Gyeonggi-do, KR;

Se Jin Kim, Seoul, KR;

Kyoung Rok Lim, Seoul, KR;

Assignee:

Hyundai Steel Company, Incheon, KR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 9/00 (2006.01); C21D 6/00 (2006.01); C22C 38/00 (2006.01); C21D 9/52 (2006.01); C21D 8/06 (2006.01); C21D 8/08 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/58 (2006.01);
U.S. Cl.
CPC ...
C21D 9/525 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/065 (2013.01); C21D 8/08 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/58 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/009 (2013.01);
Abstract

A steel reinforcing bar contains 0.06 wt % to 0.11 wt % carbon, more than 0 and not more than 0.25 wt % silicon, 0.8 wt % or more and less than 2.0 wt % manganese, more than 0 and not more than 0.01 wt % phosphorus, more than 0 and not more than 0.01 wt % sulfur, 0.01 to 0.03 wt % aluminum, 0.50 to 1.00 wt % nickel, 0.027 to 0.125 wt % molybdenum, more than 0 and not more than 0.25 wt % chromium, more than 0 and not more than 0.28 wt % copper, more than 0 and not more than 0.01 wt % nitrogen, and the remainder being iron and unavoidable impurities. The reinforcing bar has a surface layer and a core. The surface layer has a hardened layer of tempered martensite, and the core has a mixed structure of bainite, ferrite and pearlite.


Find Patent Forward Citations

Loading…