The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 13, 2023

Filed:

Oct. 02, 2019
Applicant:

Borealis Ag, Vienna, AT;

Inventors:

Susanne Kahlen, Linz, AT;

Michael Jerabek, Linz, AT;

Assignee:

BOREALIS AG, Vienna, AT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 23/12 (2006.01); C08L 23/06 (2006.01); C08L 25/06 (2006.01); C08L 33/24 (2006.01); C08J 3/00 (2006.01); C08J 3/12 (2006.01); C08J 11/18 (2006.01); C08K 3/24 (2006.01); C08K 3/34 (2006.01);
U.S. Cl.
CPC ...
C08L 23/12 (2013.01); C08J 3/005 (2013.01); C08J 3/12 (2013.01); C08J 11/18 (2013.01); C08K 3/24 (2013.01); C08K 3/346 (2013.01); C08L 23/06 (2013.01); C08L 25/06 (2013.01); C08L 33/24 (2013.01);
Abstract

A polyethylene-polypropylene composition obtainable by blending a) 80 to 97 wt.-% of a blend (A) comprising A-1) polypropylene and A-2) polyethylene, wherein the ratio of polypropylene to polyethylene is from 3:7 to 13:7, and wherein blend (A) is a recycled material, which is recovered from a waste plastic material derived from post-consumer and/or post-industrial waste; and b) 3 to 20 wt.-% of a compatibilizer (B) being a heterophasic random copolymer comprising a random polypropylene copolymer matrix phase and an elastomer phase dispersed therein, whereby the heterophasic random copolymer has—a xylene insolubles content (XCI) of from 65 to 88 wt.-% (ISO 16152, led, 25° C.), and—a xylene soluble content XCS of 12 to 35 wt.-% (ISO 16152, led, 25° C.), the XCS fraction having an intrinsic viscosity (measured in decalin according to DIN ISO 1628/1 at 135° C.) of 1.2 dl/g to less than 3.0 dl/g, and—a flexural modulus of from 300 to 600 MPa (ISO 178, measured on injection moulded specimens, 23° C.); whereby the ratio of MFR(blend (A))/MFR(compatibilizer (B)) (ISO1133, 2.16 kg load at 230° C.), is in the range of 0.5 to 1.5.