The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 13, 2023

Filed:

Feb. 01, 2021
Applicant:

Verily Life Sciences Llc, South San Francisco, CA (US);

Inventors:

Daniel B. Otts, Pleasanton, CA (US);

Stein Kuiper, South San Francisco, CA (US);

Assignee:

Verily Life Sciences LLC, South San Francisco, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
A61F 2/16 (2006.01); G02C 7/08 (2006.01); G02B 3/14 (2006.01); G02B 26/00 (2006.01); A61L 31/02 (2006.01); A61L 31/06 (2006.01); A61L 31/08 (2006.01); G02B 7/02 (2021.01); A61F 2/48 (2006.01);
U.S. Cl.
CPC ...
A61F 2/1635 (2013.01); A61L 31/022 (2013.01); A61L 31/06 (2013.01); A61L 31/088 (2013.01); G02B 3/14 (2013.01); G02B 26/005 (2013.01); G02C 7/085 (2013.01); A61F 2/482 (2021.08); A61F 2210/0014 (2013.01); A61F 2250/0001 (2013.01); A61F 2250/0002 (2013.01); A61F 2250/0003 (2013.01); A61F 2250/0018 (2013.01); A61F 2250/0056 (2013.01); G02B 7/02 (2013.01);
Abstract

Ophthalmic devices having elastic electrodes are disclosed herein. An example ophthalmic device may be an intraocular lens that includes a support structure, two optical windows, two immiscible fluids, and an elastic electrode. The support structure may have an inner surface defining an aperture with first and second optical windows disposed on opposite sides of the support structure and spanning the aperture. The two immiscible liquids may be disposed in a cavity formed by the aperture and the first and second optical windows, and the elastic electrode may be disposed on the inner surface. The elastic electrode may be formed from an elastic metal alloy having a minimum yield strain of 0.25%.