The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 06, 2023

Filed:

Sep. 04, 2018
Applicants:

Beijing Hina Battery Technology Co., Ltd., Beijing, CN;

Institute of Physics, the Chinese Academy of Sciences, Beijing, CN;

Inventors:

Yaxiang Lu, Beijing, CN;

Yongsheng Hu, Beijing, CN;

Kun Tang, Beijing, CN;

Hong Li, Beijing, CN;

Xuejie Huang, Beijing, CN;

Liquan Chen, Beijing, CN;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/04 (2006.01); H01M 4/133 (2010.01); H01M 4/1393 (2010.01); H01M 10/054 (2010.01); H01M 4/583 (2010.01); H01M 4/02 (2006.01); H01M 4/587 (2010.01);
U.S. Cl.
CPC ...
H01M 4/583 (2013.01); H01M 4/0442 (2013.01); H01M 4/133 (2013.01); H01M 4/1393 (2013.01); H01M 10/054 (2013.01); H01M 4/049 (2013.01); H01M 4/0471 (2013.01); H01M 4/587 (2013.01); H01M 2004/027 (2013.01);
Abstract

Embodiments of the present disclosure are a pitch-based negative electrode material for a sodium-ion battery and related methods and applications. The method comprises: placing a pitch recursor into a muffle furnace to allow the pitch precursor to experience pre-oxidation for 2 to 6 hours at a temperature ranging from 200° C. to 350° C., to obtain pre-oxidized pitch; placing the pre-oxidized pitch into a high-temperature carbonization furnace, and increasing the temperature to 1300° C. to 1600° C. at a temperature increase speed of 0.5° C./min to 5° C./min, and carrying out thermal treatment on the pre-oxidized pitch in an inert atmosphere for 1 to 10 hours, to allow the pre-oxidized pitch to experience carbonization reactions, oxygen in the pre-oxidized pitch being used for breaking an ordered structure of the pitch during the carbonization of the pre-oxidized pitch, so as to form a wedge-shaped voids disordered structure.