The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
May. 30, 2023
Filed:
May. 12, 2022
Beijing University of Technology, Beijing, CN;
BEIJING UNIVERSITY OF TECHNOLOGY, Beijing, CN;
Abstract
The invention discloses Method for whole component microwave fast digestion and precious metal extraction from ionic liquid of waste circuit board, and belongs to the field of hydrometallurgy. Based on the theory that microwaves can directly penetrate through a leaching medium to directly heat a circuit board, microwave-assisted leaching can reinforce mass transfer and heat transfer in the traditional leaching process, the leaching time is greatly shortened, and the leaching efficiency is improved. Before leaching, a waste circuit board does not need to be smashed, and environmental protection is achieved while energy is saved. The temperature rising process and reaction time of the reaction can be controlled, the whole process is conducted under the airtight condition, heat loss in the leaching process is avoided, the valuable leaching rate is high, the selectivity is high, and efficient leaching of valuable metal can be achieved. Precious metal leachate is extracted through imidazolium ionic liquid, the selectivity of the imidazolium ionic liquid to gold is high, and the co-extraction phenomenon of gold, nickel, copper and other ions is avoided. The method for extracting the precious metal leachate through ionic liquid is a green and clean recycling method, and the overall recycling rate of gold, nickel and copper can reach 99% or above.