The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 25, 2023

Filed:

Oct. 19, 2018
Applicant:

Corning Incorporated, Corning, NY (US);

Inventors:

Jaymin Amin, Corning, NY (US);

Benedict Osobomen Egboiyi, Painted Post, NY (US);

Jonathan David Pesansky, Corning, NY (US);

Kevin Barry Reiman, Horseheads, NY (US);

Rostislav Vatchev Roussev, Painted Post, NY (US);

Brian Paul Strines, Painted Post, NY (US);

Assignee:

Corning Incorporated, Coming, NY (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C03C 3/04 (2006.01); C03C 4/18 (2006.01); C03C 21/00 (2006.01); C03C 3/097 (2006.01); C03C 3/087 (2006.01); C03C 3/091 (2006.01); C03C 3/093 (2006.01); C03C 3/095 (2006.01); C03C 3/085 (2006.01); G06F 1/16 (2006.01); H04B 1/3827 (2015.01);
U.S. Cl.
CPC ...
C03C 21/002 (2013.01); C03C 3/04 (2013.01); C03C 3/085 (2013.01); C03C 3/087 (2013.01); C03C 3/091 (2013.01); C03C 3/093 (2013.01); C03C 3/095 (2013.01); C03C 3/097 (2013.01); C03C 4/18 (2013.01); C03C 21/00 (2013.01); G06F 1/1637 (2013.01); C03C 2204/00 (2013.01); G06F 2200/1634 (2013.01); H04B 1/3827 (2013.01); Y10T 428/315 (2015.01);
Abstract

Chemically strengthened glass articles having at least one deep compressive layer extending from a surface of the article to a depth of at least about 45 μm within the article are provided. In one embodiment, the compressive stress profile includes a single linear segment extending from the surface to the depth of compression DOC. Alternatively, the compressive stress profile includes two linear portions: the first portion extending from the surface to a relatively shallow depth and having a steep slope; and a second portion extending from the shallow depth to the depth of compression. The strengthened glass has a 60% survival rate when dropped from a height of 80 cm in an inverted ball drop test and a peak load at failure of at least 10 kgf as determined by abraded ring-on-ring testing. Methods of achieving such stress profiles are also described.