The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 18, 2023

Filed:

May. 18, 2018
Applicant:

Kao Corporation, Tokyo, JP;

Inventors:

Taichi Homma, Utsunomiya, JP;

Ryohei Suzuki, Ichikai-machi, JP;

Takahiro Maezawa, Ichikai-machi, JP;

Tetsuya Tabata, Utsunomiya, JP;

Assignee:

Kao Corporation, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 1/10 (2022.01); C06B 33/00 (2006.01); A61F 7/08 (2006.01); C09K 5/18 (2006.01); B22F 9/04 (2006.01); B22F 9/22 (2006.01); B22F 1/105 (2022.01);
U.S. Cl.
CPC ...
C09K 5/18 (2013.01); B22F 1/105 (2022.01); B22F 9/04 (2013.01); B22F 9/22 (2013.01); C06B 33/00 (2013.01); A61F 7/08 (2013.01); B22F 2009/045 (2013.01); B22F 2301/35 (2013.01);
Abstract

An iron powder for an exothermic composition according to the present invention has a bulk density of 0.3 to 1.5 g/cm. Furthermore, an exothermic composition according to the present invention contains the iron powder, a carbon material, a halide salt, and water. Furthermore, an exothermic body production method according to the present invention includes: forming a coated member by coating a base material sheet with a flowable exothermic composition containing the iron powder, a carbon material, and water; and adjusting an amount of moisture in the coated member by removing water from the coated member. Furthermore, the present invention is directed to a production method for the iron powder (an iron powder for an exothermic composition) including: a reducing step of reducing iron oxide to obtain reduced iron; and a step of milling the reduced iron. In the reducing step, the iron oxide is reduced by introducing iron oxide and a solid reductant with a volatile matter content of 10% by mass or more into a heating furnace whose internal portion contains no sulfur gas or is set to an air or inert gas atmosphere, and setting the internal portion to a reducing gas atmosphere through heating under a condition that an ambient temperature of the internal portion is from 900 to 1000° C.