The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 31, 2023

Filed:

Nov. 15, 2018
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Anirban Chakraborty, Chesterton, IN (US);

Hassan Ghassemi-Armaki, Schererville, IN (US);

Pascal Bertho, Maizieres-les-Metz, FR;

Christian Allely, Metz, FR;

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/58 (2006.01); C21D 1/76 (2006.01); C21D 9/46 (2006.01); C21D 9/56 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/44 (2006.01); C22C 38/48 (2006.01); C22C 38/50 (2006.01); C22C 38/54 (2006.01); C23C 2/06 (2006.01); B23K 103/04 (2006.01); B23K 11/11 (2006.01); B23K 35/02 (2006.01); B23K 35/28 (2006.01); B23K 35/30 (2006.01);
U.S. Cl.
CPC ...
C22C 38/58 (2013.01); C21D 1/76 (2013.01); C21D 9/46 (2013.01); C21D 9/561 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/44 (2013.01); C22C 38/48 (2013.01); C22C 38/50 (2013.01); C22C 38/54 (2013.01); C23C 2/06 (2013.01); B23K 11/11 (2013.01); B23K 35/0255 (2013.01); B23K 35/286 (2013.01); B23K 35/3073 (2013.01); B23K 2103/04 (2018.08);
Abstract

The present invention relates to a method for the manufacture of a coated steel sheet comprising the following successive steps: A. the coating of the steel sheet with a first coating consisting of nickel and having a thickness between 600 nm and 1400 nm, the steel sheet having the following composition in weight: 0.10<C<0.40%, 1.5<Mn<3.0%, 0.7<Si<3.0%, 0.05<Al<1.0%, 0.75<(Si+Al)<3.0%, and on a purely optional basis, one or more elements such as Nb≤0.5%, B≤0.010%, Cr≤1.0%, Mo≤0.50%, Ni≤1.0%, Ti≤0.5%, the remainder of the composition making up of iron and inevitable impurities resulting from the elaboration, B. the recrystallization annealing at a temperature between 820 to 1200° C., C. the coating with a second coating based on zinc not comprising nickel.


Find Patent Forward Citations