The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 17, 2023

Filed:

Jan. 10, 2017
Applicant:

Sika Hamatite Co., Ltd., Hiratsuka, JP;

Inventors:

Megumi Abe, Hiratsuka, JP;

Yuichi Matsuki, Hiratsuka, JP;

Assignee:

Sika Hamatite Co., Ltd., Kanagawa, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B29C 65/52 (2006.01); B32B 27/32 (2006.01); B32B 37/06 (2006.01); B29C 59/16 (2006.01); B32B 38/00 (2006.01); B32B 37/12 (2006.01); C09J 5/00 (2006.01); C09J 201/00 (2006.01); B29C 59/14 (2006.01); B29C 59/08 (2006.01); B29C 48/08 (2019.01); C09J 5/06 (2006.01); B29C 35/08 (2006.01); B32B 7/12 (2006.01); B32B 27/36 (2006.01);
U.S. Cl.
CPC ...
B29C 65/522 (2013.01); B29C 48/08 (2019.02); B29C 59/08 (2013.01); B29C 59/14 (2013.01); B29C 59/16 (2013.01); B29C 65/52 (2013.01); B32B 27/32 (2013.01); B32B 37/06 (2013.01); B32B 37/12 (2013.01); B32B 38/0008 (2013.01); C09J 5/00 (2013.01); C09J 5/06 (2013.01); C09J 201/00 (2013.01); B29C 2035/0827 (2013.01); B32B 7/12 (2013.01); B32B 27/36 (2013.01); B32B 2038/0048 (2013.01);
Abstract

A method for producing a multilayer member having a first member containing a crystallizable thermoplastic resin, an adhesion layer, and a second member includes performing a dry treatment on a surface of the first member containing a crystallizable thermoplastic resin so as to satisfy conditions A and B, applying an adhesive to the surface of the first member to form an adhesive layer on the surface, and adhering the second member to the adhesive layer. (A) The ultimate temperature of the first member is lower than the peak temperature of endothermic peak obtained by DSC of the crystallizable thermoplastic resin. (B) The high temperature holding time of the first member is less than 3.0 seconds, which is when the first member is continuously held at a temperature not lower than a temperature at the starting point of the endothermic peak obtained by DSC of the crystallizable thermoplastic resin.