The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 06, 2022

Filed:

Feb. 04, 2020
Applicant:

Toyota Jidosha Kabushiki Kaisha, Toyota, JP;

Inventor:

Shingo Komura, Nagakute, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/36 (2006.01); H01M 4/62 (2006.01); H01M 4/485 (2010.01); H01M 4/04 (2006.01); H01M 10/0562 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/366 (2013.01); H01M 4/0404 (2013.01); H01M 4/0471 (2013.01); H01M 4/485 (2013.01); H01M 4/625 (2013.01); H01M 10/0562 (2013.01); H01M 2004/028 (2013.01); H01M 2300/0068 (2013.01);
Abstract

In conventional arts, it is impossible to form a good solid-solid interface in cathode mixture layers of all-solid-state batteries, which significantly deteriorates resistance of the all-solid-state battery after the charge/discharge cycle, which is problematic. A cathode slurry is produced by a method including: a first step of dispersing a conductive additive constituted of carbon in a solvent to obtain a first slurry; a second step of dispersing a sulfide solid electrolyte in the first slurry to obtain a second slurry; and a third step of dispersing a cathode active material in the second slurry to obtain a third slurry, to be used to form a cathode mixture layer. This may suppress agglomeration of the cathode active material as using the conductive additive as a core, and may lower the proportion of agglomerate present in the cathode mixture layer. As a result, a good solid-solid interface may be formed in the cathode mixture layer of the all-solid-state battery, and the resistance increase of the all-solid-state battery after the charge/discharge cycle may be suppressed.