The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 06, 2022

Filed:

Oct. 04, 2018
Applicant:

Posco, Pohang-si, KR;

Inventor:

Jin-Ho Bae, Gwangyang-si, KR;

Assignee:

POSCO HOLDINGS INC., Seoul, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/32 (2006.01); B23K 11/00 (2006.01); B23K 35/02 (2006.01); B23K 35/30 (2006.01); C21D 8/02 (2006.01); C21D 8/10 (2006.01); C21D 9/08 (2006.01); C22C 38/00 (2006.01); C22C 38/06 (2006.01); C22C 38/20 (2006.01); C22C 38/26 (2006.01); C22C 38/28 (2006.01); B23K 103/04 (2006.01);
U.S. Cl.
CPC ...
C22C 38/32 (2013.01); B23K 11/002 (2013.01); B23K 35/0233 (2013.01); B23K 35/3073 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/105 (2013.01); C21D 9/08 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/06 (2013.01); C22C 38/20 (2013.01); C22C 38/26 (2013.01); C22C 38/28 (2013.01); B23K 2103/04 (2018.08); C21D 2211/001 (2013.01);
Abstract

A preferable aspect of the present invention provides a hot-rolled steel sheet with excellent low-temperature toughness, a steel pipe using the same, and a manufacturing method therefor, wherein the hot-rolled steel sheet contains, by weight, 0.35-0.65% C, 0.01-0.4% Si, 13-26% Mn, 0.01-0.3% Ti, 0.01% or less B, 4% or less Al, 1-6% Cr, 0.05% or less P, 0.02% or less S, 0.01% or less N, 0.01-2% Cu, 0.001-0.015% Nb, and the balance Fe and other unavoidable impurities, the alloy elements satisfying the following relational formulas—[Relational formula 1] 70<[10*(C/12)+(Mn/55)+(Al/27)]*100<95 and [Relational formula 2] 4<100*(Cr/52+100*(Nb/93))<9; wherein a microstructure comprises, by area fraction, 97% or more (including 100%) of austenite and 3% or less (including 0%) of a carbide, the crystal grain size of the austenite being 18-30 μm or less; and wherein the size of the carbide is 0.5 μm or less.