The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 18, 2022

Filed:

Jun. 18, 2014
Applicant:

Constellium Issoire, Issoire, FR;

Inventors:

Armelle Danielou, Les Echelles, FR;

Gaelle Pouget, Grenoble, FR;

Christophe Sigli, Grenoble, FR;

Assignee:

Constellium Issoire, Issoire, FR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B64C 3/26 (2006.01); C22F 1/057 (2006.01); C22C 21/12 (2006.01); B22D 21/00 (2006.01); C21D 1/30 (2006.01); C21D 8/00 (2006.01); C22C 1/02 (2006.01); C22C 21/14 (2006.01); C22C 21/16 (2006.01);
U.S. Cl.
CPC ...
B64C 3/26 (2013.01); B22D 21/007 (2013.01); C21D 1/30 (2013.01); C21D 8/00 (2013.01); C22C 1/026 (2013.01); C22C 21/12 (2013.01); C22C 21/14 (2013.01); C22C 21/16 (2013.01); C22F 1/057 (2013.01);
Abstract

Extrados structural element made from an aluminum, copper and lithium alloy and method for manufacturing same. An alloy with composition (in wt %) 4.2-5.2 Cu, 0.9-1.2 Li, 0.1-0.3 Ag, 0.1-0.25 Mg, 0.08-0.18 Zr, 0.01-0.15 Ti, an Fe and Si content level less than or equal to 0.1% each, and other element with content level less than or equal to 0.05% each and 0.15% in total, is poured, homogenized, deformed hot, placed in a solution at a temperature of at least 515° C., pulled from 0.5 to 5% and annealed. The combination of magnesium, copper and manganese content with the temperature in solution can reach an advantageous elasticity under compression limit. Products having a thickness of at least 12 mm have, in the longitudinal direction, an elasticity under compression limit of at least 645 MPa and an elongation of at least 7%.