The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 11, 2022

Filed:

Feb. 21, 2020
Applicant:

Furukawa Electric Co., Ltd., Tokyo, JP;

Inventors:

Jirou Hiroishi, Tokyo, JP;

Hidekazu Hara, Tokyo, JP;

Yuka Sawada, Tokyo, JP;

Masami Tazuke, Tokyo, JP;

Toshihiro Suzuki, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 23/06 (2006.01); C08K 3/08 (2006.01); C08K 7/02 (2006.01); C08L 23/12 (2006.01); C08L 67/02 (2006.01); C08L 79/06 (2006.01); G01N 3/56 (2006.01); C08L 1/02 (2006.01);
U.S. Cl.
CPC ...
C08L 23/06 (2013.01); C08K 3/08 (2013.01); C08K 7/02 (2013.01); C08L 1/02 (2013.01); C08L 23/12 (2013.01); C08L 67/02 (2013.01); C08L 79/06 (2013.01); G01N 3/56 (2013.01); C08K 2003/0812 (2013.01); C08K 2201/004 (2013.01); C08L 2205/16 (2013.01); C08L 2207/066 (2013.01); C08L 2207/20 (2013.01);
Abstract

A cellulose-fiber-dispersing polyolefin resin composite material, containing a polyolefin resin and a cellulose fiber dispersed in the polyolefin resin, in which the composite material contains the cellulose fiber of 3 mass % or more and less than 70 mass %, and when the composite material is subjected to the abrasion test according to ISO 6722 under the following test conditions, the amount of abrasion after 5,000 reciprocations satisfies the [Formula 1]: (Amount of abrasion [mm] of the cellulose-fiber-dispersing polyolefin resin composite material)<−0.003×(Cellulose effective mass ratio of the cellulose-fiber-dispersing polyolefin resin composite material)+0.3, [Test Conditions for Abrasion Test] Load: 1.7 kg, Needle diameter: φ0.45 mm, Stroke length: 10 mm, Period: 60 reciprocations/min, Test piece: length 38 mm×width 6 mm×thickness 1 mm, Temperature: 23° C.


Find Patent Forward Citations