The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Sep. 27, 2022
Filed:
Sep. 13, 2017
Thyssenkrupp Steel Europe Ag, Duisburg, DE;
Thyssenkrupp Ag, Essen, DE;
Frank Friedel, Dortmund, DE;
Friedhelm Macherey, Alpen, DE;
Lena Sattler, Krefeld, DE;
Robert Yanik, Moers, DE;
ThyssenKrupp Steel Europe AG, Duisburg, DE;
thyssenkrupp AG, Essen, DE;
Abstract
A flat steel product which, following a 5% biaxial deformation, exhibits, on one surface, a Wsa(1-5) value of <0.35 μm, a planar anisotropy Δr of −0.5 to +0.5 and, from the surface to a depth of <200 μm, and a nanohardness of >0.1 to <3.0 GPa. Also, a method of making the product where a slab including (in wt. %) 0.0003-0.050% C, 0.0001-0.20% Si, 0.01-1.5% Mn, 0.001-0.10% P, 0.0005-0.030% S, 0.001-0.12% AI, and 0.0001-0.01% N, the remainder Fe and impurities is heated to 1200-1270° C., rough-rolled with a reduction of 80-90%, and finish-hot-rolled at 850-950° C. with a reduction of 85-95%, for a total deformation of 95-99.5%. The reduction in the last hot roll pass is 1-25%, and the product is cooled at 4-30 K/s to a coiling temperature of 620-780° C. Following pickling, the product is cold-rolled with a total degree of deformation of 70-90% and recrystallization annealed at 650-900° C.