The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 20, 2022

Filed:

Oct. 04, 2017
Applicant:

Solar Paste, Llc, Wilmington, DE (US);

Inventors:

Dave Hui, Bristol, GB;

Michael Stephen Wolfe, Wilmington, DE (US);

Howard David Glicksman, Durham, NC (US);

Haixin Yang, Durham, NC (US);

Takashi Hinotsu, Tokyo, JP;

Shingo Teragawa, Tokyo, JP;

Assignee:

SOLAR PASTE, LLC, Wilmington, DE (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
H01B 1/22 (2006.01); B22F 9/24 (2006.01); B05D 3/02 (2006.01); H01B 13/00 (2006.01); B22F 1/10 (2022.01); C22C 5/06 (2006.01); C22C 1/04 (2006.01); B22F 7/04 (2006.01); H05K 1/09 (2006.01); B22F 1/102 (2022.01); B22F 1/0545 (2022.01);
U.S. Cl.
CPC ...
H01B 1/22 (2013.01); B05D 3/0254 (2013.01); B22F 1/10 (2022.01); B22F 9/24 (2013.01); H01B 13/0016 (2013.01); H01B 13/0036 (2013.01); B22F 1/0545 (2022.01); B22F 1/102 (2022.01); B22F 2007/047 (2013.01); B22F 2301/255 (2013.01); B22F 2304/05 (2013.01); B22F 2998/10 (2013.01); B22F 2999/00 (2013.01); C22C 1/0466 (2013.01); C22C 5/06 (2013.01); H05K 1/097 (2013.01); H05K 2203/1131 (2013.01);
Abstract

This disclosure relates to a method of manufacturing an electrically conductive thick film comprising steps of: (a) applying a fine silver particle dispersion on a substrate, wherein the fine silver particle dispersion comprises, (i) 60 to 95 wt. % of fine silver particles, wherein particle diameter (D50) of the fine silver particles is 50 to 300 nm, (ii) 4.5 to 39 wt. % of a solvent; and (iii) 0.1 to 3 wt. % of a resin, wherein the glass transition temperature (Tg) of the resin is 70 to 300° C., wherein the weight percentages are based on the weight of the fine silver particle dispersion; and (b) heating the applied fine silver particle dispersion at 80 to 1000° C.