The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 20, 2022

Filed:

Aug. 25, 2017
Applicants:

Fukuda Metal Foil & Powder Co., Ltd., Kyoto, JP;

Technology Research Association for Future Additive Manufacturing, Tokyo, JP;

Inventors:

Seiichi Matsumoto, Kyoto, JP;

Yuji Sugitani, Kyoto, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
G01N 11/14 (2006.01); B33Y 30/00 (2015.01); B33Y 50/00 (2015.01); B23K 26/342 (2014.01); B23K 15/00 (2006.01);
U.S. Cl.
CPC ...
G01N 11/14 (2013.01); B23K 15/0086 (2013.01); B23K 26/342 (2015.10); B33Y 30/00 (2014.12); B33Y 50/00 (2014.12);
Abstract

This invention relates to a method of evaluating powder for lamination shaping by stable criteria. In this method, it is evaluated whether powder for lamination shaping can be spread into a uniform powder layer in the lamination shaping, wherein the powder is evaluated using, as a flowability of the powder, an adhesive force of the powder calculated from a failure envelope obtained by a shear test. The shear test is conducted by a powder rheometer, and the adhesive force is obtained from the relationship between a normal stress and a shearing stress at the powder rheometer. If the adhesive force is 0.450 kPa or less, the powder is evaluated to be spread into a uniform powder layer in the lamination shaping. Furthermore, if at least one of that the 50% particle size of the powder obtained by a laser diffraction method is 3 to 250 μm and that the apparent density of the powder is 3.5 g/cmor more is satisfied, the powder is evaluated to be spread into a uniform powder layer in the lamination shaping.