The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 13, 2022

Filed:

Sep. 12, 2019
Applicant:

The Goodyear Tire & Rubber Company, Akron, OH (US);

Inventors:

Jennifer Lyn Ryba, Akron, OH (US);

Philip Jordan Young, Twinsburg, OH (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 7/00 (2006.01); B60C 1/00 (2006.01); C08K 3/36 (2006.01);
U.S. Cl.
CPC ...
C08L 7/00 (2013.01); B60C 1/0016 (2013.01); C08K 3/36 (2013.01); C08L 2205/025 (2013.01); C08L 2205/035 (2013.01); C08L 2205/06 (2013.01); C08L 2207/322 (2013.01);
Abstract

The present invention is directed to a pneumatic tire comprising a vulcanizable rubber composition, the vulcanization rubber composition comprising: 1) 100 parts by weight of elastomer consisting of 25 to 35 phr of a styrene-butadiene rubber, 25 to 35 phr of a polybutadiene, and 35 to 45 phr of a natural rubber or synthetic polyisoprene, wherein the styrene-butadiene rubber is a functionalized solution polymerized styrene-butadiene elastomer having a glass transition temperature Tg(A) ranging from −30 to −10° C. and having at least one functional group; the natural rubber or synthetic polyisoprene has a Tg(B) ranging from −60 to −70° C.; and the polybutadiene is a cis 1,4 polybutadiene having a Tg(C) ranging from −110 to −90° C., wherein Tg(A)−Tg(B)≥25° C., and Tg(B)−Tg(C)≥25° C.; 2) 60 to 80 phr of a prehydrophobated silica; 3) 1 to 10 phr of carbon black; 4) 1 to 3 phr of rubber processing oil; and 5) 5 to 25 phr of at least one hydrocarbon resin having a Tg≥20° C., wherein the weight ratio of hydrocarbon resin to rubber processing oil is greater than 8.