The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 23, 2022

Filed:

May. 10, 2019
Applicant:

Lg Electronics Inc., Seoul, KR;

Inventors:

Sanghyun Hong, Seoul, KR;

Jihyun Kim, Seoul, KR;

Seojin Lee, Seoul, KR;

Sangeun Shim, Seoul, KR;

Jiyoung Jung, Seoul, KR;

Sosan Hwang, Seoul, KR;

Yooseok Kwon, Seoul, KR;

Assignee:

LG ELECTRONICS INC., Seoul, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 9/00 (2006.01); B22F 9/24 (2006.01); C01G 39/02 (2006.01); C01G 41/02 (2006.01); B22F 1/054 (2022.01); B22F 1/142 (2022.01);
U.S. Cl.
CPC ...
B22F 9/24 (2013.01); B22F 1/054 (2022.01); B22F 1/142 (2022.01); C01G 39/02 (2013.01); C01G 41/02 (2013.01); B22F 2202/03 (2013.01); B22F 2302/25 (2013.01); B22F 2304/058 (2013.01);
Abstract

The present invention provides a method for the manufacture of transition metal oxide fine particles, the method comprising the steps of: heating a strong-alkaline aqueous solution while stirring same; adding to and dissolving in the heated strong-alkaline aqueous solution a transition metal oxide; adding a strong-acid aqueous solution to the strong alkaline aqueous solution in which the transition metal oxide is dissolved, while stirring same, thereby re-dissolving a solid generated at the interface between the strong-alkaline aqueous solution and the strong-acid aqueous solution; adjusting the pH of the mixed aqueous solution resulting from mixing the strong-alkaline aqueous solution and the strong acid aqueous solution, through adjustment of the adding rate and amount of the strong-acid aqueous solution, to precipitate transition metal oxide fine particles; and separating the transition metal oxide fine particles from the mixed aqueous solution and sequentially washing, drying, and thermally treating the separated transition metal oxide fine particles.