The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 16, 2022

Filed:

Mar. 16, 2020
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventors:

Jin Seok Byun, Daejeon, KR;

Heon Kim, Daejeon, KR;

Boo Kyung Kim, Daejeon, KR;

Seok Hoon Jang, Daejeon, KR;

Yeong Rae Chang, Daejeon, KR;

Assignee:

LG CHEM, LTD., Seoul, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
G02B 1/111 (2015.01); G02B 1/14 (2015.01); B32B 27/08 (2006.01); C08J 7/043 (2020.01); C08J 7/044 (2020.01); C08J 7/046 (2020.01); C08J 7/04 (2020.01); C09D 4/00 (2006.01); C08K 3/36 (2006.01); C08K 7/26 (2006.01); B32B 5/14 (2006.01); B32B 5/16 (2006.01);
U.S. Cl.
CPC ...
G02B 1/111 (2013.01); B32B 5/145 (2013.01); B32B 5/16 (2013.01); B32B 27/08 (2013.01); C08J 7/042 (2013.01); C08J 7/043 (2020.01); C08J 7/044 (2020.01); C08J 7/046 (2020.01); C09D 4/00 (2013.01); G02B 1/14 (2015.01); C08J 2301/02 (2013.01); C08J 2435/02 (2013.01); C08K 3/36 (2013.01); C08K 7/26 (2013.01);
Abstract

Described herein is an anti-reflective film including: a hard coating layer; and a low-refractive layer containing a binder resin and hollow inorganic nanoparticles and solid inorganic nanoparticles dispersed in the binder resin. The hollow and solid inorganic particles are dispersed in the low-refractive layer such that the amount of the solid inorganic nanoparticles positioned close to an interface between the hard coating layer and the low-refractive layer is larger than that of the hollow inorganic nanoparticles. Also described is a manufacturing method of the anti-reflective film including: applying a resin composition containing a photopolymerizable compound or a (co)polymer thereof, a fluorine-containing compound including a photoreactive functional group, a photoinitiator, hollow inorganic nanoparticles, and solid inorganic nanoparticles on a hard coating layer, and drying the applied resin composition at a temperature of 35° C. to 100° C.; and photocuring the dried resin composition.