The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 16, 2022

Filed:

Jul. 29, 2016
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Tiago Machado Amorim, Longeville les Metz, FR;

Christian Allely, Metz, FR;

Grégory Leuillier, Hagondange, FR;

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C23C 2/12 (2006.01); C23C 2/06 (2006.01); C23C 2/28 (2006.01); C21D 1/673 (2006.01); C21D 8/02 (2006.01); C22C 21/10 (2006.01); C22F 1/053 (2006.01); C23C 22/07 (2006.01);
U.S. Cl.
CPC ...
C23C 2/12 (2013.01); C21D 1/673 (2013.01); C21D 8/0257 (2013.01); C23C 2/06 (2013.01); C23C 2/28 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

A method for the manufacture of a hardened part coated with a phosphatable coating is provided. The method includes providing a steel sheet pre-coated with a metallic coating including from 4.0 to 20.0% by weight of zinc, from 1.0 to 3.5% by weight of silicon, optionally from 1.0 to 4.0% by weight of magnesium, and optionally additional elements chosen from Pb, Ni, Zr, or Hf, the content by weight of each additional element being less than 0.3% by weight, the balance being aluminum and unavoidable impurities and residuals elements. The steel sheet is cut to obtain a blank, the blank is thermally treated at a temperature between 840 and 950° C. to obtain a fully austenitic microstructure in the steel, the blank is transferred into a press tool and hot-formed to obtain a part. The part is cooled to obtain a martensitic or martensitic-bainitic microstructure or made of at least 75% of equiaxed ferrite, from 5 to 20% of martensite and bainite in amount less than or equal to 10%.