The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 09, 2022

Filed:

May. 10, 2018
Applicants:

Nippon Steel Corporation, Tokyo, JP;

Vallourec Oil and Gas France, Aulnoye-Aymeries, FR;

Inventors:

Masanari Kimoto, Tokyo, JP;

Masahiro Oshima, Tokyo, JP;

Assignees:

Nippon Steel Corporation, Tokyo, JP;

Vallourec Oil and Gas France, Aulnoye-Aymeries, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
F16L 58/08 (2006.01); C23C 22/30 (2006.01); C25D 3/22 (2006.01); C23C 22/77 (2006.01); C23C 28/02 (2006.01); C25D 7/04 (2006.01); F16L 15/00 (2006.01); C22C 18/00 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01);
U.S. Cl.
CPC ...
F16L 58/08 (2013.01); C23C 22/30 (2013.01); C23C 22/77 (2013.01); C23C 28/021 (2013.01); C25D 3/22 (2013.01); C25D 7/04 (2013.01); F16L 15/006 (2013.01); C22C 18/00 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C23C 2222/10 (2013.01);
Abstract

This invention provides a threaded connection for oil country tubular goods that exhibits excellent corrosion resistance and galling resistance, and a method for producing the threaded connection for oil country tubular goods. The method includes a Zn—Ni alloy plating layer formation step of forming a Zn—Ni alloy plating layer, and a chromate coating formation step of forming a chromate coating after the Zn—Ni alloy plating layer formation step. The chromate coating formation step includes a chromate treatment step and a drying step. The chromate coating formation step satisfy one or more conditions selected from the following conditions 1 to 3. Condition 1: stirring speed of the chromating solution in the chromate treatment step: a linear speed of 0.5 m/s or more; Condition 2: chromate treatment time in the chromate treatment step: less than 50 seconds; and Condition 3: drying temperature in the drying step: 60° C. or less.


Find Patent Forward Citations