The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 19, 2022

Filed:

Nov. 20, 2017
Applicant:

Korea Hydro & Nuclear Power Co., Ltd, Gyeongsangbuk-do, KR;

Inventors:

Young Hwan Hwang, Daejeon, KR;

Seok Ju Hwang, Daejeon, KR;

Cheon Woo Kim, Daejeon, KR;

Assignee:

KOREA HYDRO & NUCLEAR POWER CO., LTD, Gyeongsangbuk-do, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H05B 6/22 (2006.01); F27D 11/12 (2006.01); C01B 33/42 (2006.01); C01F 7/02 (2022.01); C01G 25/02 (2006.01); F27B 14/06 (2006.01); F27D 1/00 (2006.01); F27D 1/12 (2006.01); G21F 9/30 (2006.01); H05B 6/28 (2006.01); F27B 14/08 (2006.01); F27B 14/10 (2006.01); F27D 9/00 (2006.01);
U.S. Cl.
CPC ...
F27D 11/12 (2013.01); C01B 33/42 (2013.01); C01F 7/02 (2013.01); C01G 25/02 (2013.01); F27B 14/061 (2013.01); F27D 1/00 (2013.01); F27D 1/12 (2013.01); G21F 9/305 (2013.01); H05B 6/28 (2013.01); F27B 2014/0837 (2013.01); F27B 2014/0843 (2013.01); F27B 2014/108 (2013.01); F27D 2001/0046 (2013.01); F27D 2009/001 (2013.01);
Abstract

A metal oxide barrier and a connecting method for solving the problems in which sectors of an existing cold crucible are connected by means of a mica plate and the mica plate is damaged due to arcing and the like and in which the sectors are strongly connected by means of the mica plate and thus are difficult to replace and maintain. A cold crucible, comprising a metal oxide barrier, according to the present invention can prevent arcing, enables reduction of damage on the edge part of a water cooling sector due to a molten material and thus enhances durability. Moreover, the metal oxide barrier can easily be replaced compared to an existing mica plate and thus enables easy maintenance and repair.