The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 12, 2022

Filed:

Mar. 05, 2019
Applicant:

Toyota Jidosha Kabushiki Kaisha, Toyota, JP;

Inventors:

Koji Torita, Nagoya, JP;

Akihiro Ochiai, Toyonaka, JP;

Yusuke Fukumoto, Toyonaka, JP;

Harunari Shimamura, Toyonaka, JP;

Takuya Asari, Osaka, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/66 (2006.01); H01M 4/131 (2010.01); H01M 4/525 (2010.01); H01M 4/36 (2006.01); H01M 4/62 (2006.01); H01M 4/485 (2010.01); H01M 4/04 (2006.01); H01M 4/1391 (2010.01); H01M 10/0525 (2010.01); H01M 10/42 (2006.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/667 (2013.01); H01M 4/043 (2013.01); H01M 4/131 (2013.01); H01M 4/1391 (2013.01); H01M 4/366 (2013.01); H01M 4/485 (2013.01); H01M 4/525 (2013.01); H01M 4/624 (2013.01); H01M 4/625 (2013.01); H01M 4/626 (2013.01); H01M 4/661 (2013.01); H01M 4/664 (2013.01); H01M 10/0525 (2013.01); H01M 10/4235 (2013.01); H01M 2004/028 (2013.01);
Abstract

A positive electrode includes at least a positive electrode current collector, a conductive material, and a positive electrode active material. The positive electrode active material is disposed on a surface of the positive electrode current collector. The positive electrode current collector includes an aluminum foil and an aluminum oxide hydrate film. The aluminum oxide hydrate film covers a surface of the aluminum foil. The aluminum oxide hydrate film has a thickness not smaller than 10 nm and not greater than 500 nm. The aluminum oxide hydrate film has a porosity not lower than 10% and not higher than 50%. At least part of the conductive material is disposed within pores in the aluminum oxide hydrate film.


Find Patent Forward Citations

Loading…