The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 05, 2022

Filed:

Jun. 30, 2020
Applicant:

Korea Institute of Energy Research, Daejeon, KR;

Inventors:

Gu-gon Park, Daejeon, KR;

Hyun-uk Park, Seoul, KR;

Won-yong Lee, Daejeon, KR;

Sung-dae Yim, Daejeon, KR;

Min-jin Kim, Daejeon, KR;

Young-jun Sohn, Daejeon, KR;

Byungchan Bae, Daejeon, KR;

Seung-gon Kim, Daejeon, KR;

Dongwon Shin, Sejong-si, KR;

Hwanyeong Oh, Daejeon, KR;

Seung Hee Woo, Daejeon, KR;

So Jeong Lee, Daejeon, KR;

Hyejin Lee, Daejeon, KR;

Yoon Young Choi, Sejong-si, KR;

Seok-hee Park, Daejeon, KR;

Tae-hyun Yang, Daejeon, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22F 9/24 (2006.01); B22F 9/04 (2006.01); B22F 1/07 (2022.01); B22F 1/14 (2022.01); B82Y 40/00 (2011.01); B82Y 30/00 (2011.01);
U.S. Cl.
CPC ...
B22F 9/04 (2013.01); B22F 1/07 (2022.01); B22F 1/14 (2022.01); B22F 9/24 (2013.01); B22F 2201/02 (2013.01); B22F 2202/11 (2013.01); B22F 2203/00 (2013.01); B22F 2301/10 (2013.01); B22F 2301/15 (2013.01); B22F 2301/20 (2013.01); B22F 2301/35 (2013.01); B22F 2304/054 (2013.01); B22F 2998/10 (2013.01); B82Y 30/00 (2013.01); B82Y 40/00 (2013.01);
Abstract

The present disclosure is related to a method to control sizes of core-shell nanoparticles comprising the steps of: manufacturing slurry by irradiating ultrasonic waves to a dispersion solution containing a reducing solvent, a carbon support, a transition metal precursor and a precious metal precursor; manufacturing a solid by filtering the manufactured slurry, followed by washing and drying; and manufacturing a nanoparticle of a transition metal core and a platinum shell by heat-treating the dried solid at a temperature of 450 to 900° C. and a pressure of 1 to 90 bar for 0.5 to 10 hours under Natmosphere.