The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 05, 2022

Filed:

Dec. 05, 2019
Applicant:

GM Global Technology Operations Llc, Detroit, MI (US);

Inventors:

Ming Yang, Novi, MI (US);

Se H. Oh, Troy, MI (US);

Gongshin Qi, Troy, MI (US);

Wei Li, Troy, MI (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 21/04 (2006.01); B01J 23/10 (2006.01); B01J 23/46 (2006.01); B01J 23/63 (2006.01); B01J 23/72 (2006.01); B01J 23/83 (2006.01); B01J 35/10 (2006.01); B01J 37/02 (2006.01); B01J 37/03 (2006.01); B01J 37/10 (2006.01); B01D 53/94 (2006.01);
U.S. Cl.
CPC ...
B01J 23/63 (2013.01); B01D 53/945 (2013.01); B01J 21/04 (2013.01); B01J 23/10 (2013.01); B01J 23/464 (2013.01); B01J 23/72 (2013.01); B01J 23/83 (2013.01); B01J 35/1014 (2013.01); B01J 37/0207 (2013.01); B01J 37/035 (2013.01); B01J 37/105 (2013.01);
Abstract

Methods for preparing catalytic systems include passivating a gamma-phase alumina support body to yield a theta-phase alumina support body and applying catalytic metal to passivated theta-phase alumina support body. Passivating can include heating, optionally in the presence of steam. The gamma-phase alumina can be lanthanum-doped gamma-phase alumina and can be about 0.1-55 wt. % lanthanum. The catalytic metal can include rhodium, copper, or nickel. The catalytic metal can be rhodium or nickel, and the catalytic metal can be applied to the passivated theta-phase alumina support body at a loading of about 0.1-10 wt. %. The catalytic metal can be copper, and the catalytic metal can be applied to the passivated theta-phase alumina support body at a loading of about 0.1-30 wt. %. The gamma-phase alumina support body can be at least about 90 wt. % gamma-phase alumina. The passivated theta-phase alumina support body can be at least about 80 wt. % theta-phase alumina.


Find Patent Forward Citations

Loading…