The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 05, 2022

Filed:

Apr. 26, 2018
Applicant:

Kawasaki Jukogyo Kabushiki Kaisha, Kobe, JP;

Inventors:

Masahiro Negami, Kobe, JP;

Takeshi Okumura, Kobe, JP;

Ikuo Shimomura, Kobe, JP;

Katsuhiro Yoshizawa, Akashi, JP;

Yoshimichi Nomura, Kobe, JP;

Kazuo Tanaka, Kobe, JP;

Shohei Nishibe, Kobe, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01D 53/08 (2006.01); B01J 20/22 (2006.01); B01D 53/62 (2006.01); B01J 20/26 (2006.01); B01D 53/83 (2006.01); B01D 53/96 (2006.01); B01J 20/08 (2006.01); B01J 20/24 (2006.01); B01J 20/28 (2006.01); B01J 20/32 (2006.01); B01J 20/34 (2006.01);
U.S. Cl.
CPC ...
B01J 20/26 (2013.01); B01D 53/62 (2013.01); B01D 53/83 (2013.01); B01D 53/96 (2013.01); B01J 20/08 (2013.01); B01J 20/22 (2013.01); B01J 20/24 (2013.01); B01J 20/2803 (2013.01); B01J 20/28004 (2013.01); B01J 20/28028 (2013.01); B01J 20/3204 (2013.01); B01J 20/3246 (2013.01); B01J 20/3293 (2013.01); B01J 20/3425 (2013.01); B01J 20/3466 (2013.01); B01D 2253/104 (2013.01); B01D 2253/202 (2013.01); B01D 2253/25 (2013.01); B01D 2257/504 (2013.01);
Abstract

A method for manufacturing a carbon dioxide adsorbent includes: forming a kneaded product containing a hydrophilic fiber, a powdery porous material, and an aqueous hydrophilic binder dispersion into particles and drying the particles to generate porous material particles containing the hydrophilic fiber and the powdery porous material combined by the hydrophilic binder; and preparing an aqueous amine solution having an amine concentration of 5% or more and 70% or less and a temperature of 10° C. or higher and 100° C. or lower, impregnating the aqueous amine solution into the porous material particles, and aeration-drying the porous material particles impregnating the amine. The carbon dioxide adsorbent contains the porous material particles and the amine carried by the porous material particles, the porous material particles containing the hydrophilic fiber and the powdery porous material combined by the hydrophilic binder.