The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 28, 2022

Filed:

May. 24, 2019
Applicant:

Kingfa Sci. & Tech. Co., Ltd., Guangdong, CN;

Inventors:

Chunping Ouyang, Guangdong, CN;

Jian Jiao, Guangdong, CN;

Kaijin Mai, Guangdong, CN;

Xueteng Dong, Guangdong, CN;

Hui Yang, Guangdong, CN;

Weida Qu, Guangdong, CN;

Kai Xiong, Guangdong, CN;

Changli Lu, Guangdong, CN;

Xiangbin Zeng, Guangdong, CN;

Tongmin Cai, Guangdong, CN;

Xianbo Huang, Guangdong, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 67/02 (2006.01); C08L 3/02 (2006.01); C08J 5/18 (2006.01); C08K 3/26 (2006.01); C08K 3/34 (2006.01); C08K 5/053 (2006.01);
U.S. Cl.
CPC ...
C08L 67/02 (2013.01); C08J 5/18 (2013.01); C08K 3/26 (2013.01); C08K 3/34 (2013.01); C08K 5/053 (2013.01); C08L 3/02 (2013.01); C08J 2367/02 (2013.01); C08J 2403/02 (2013.01); C08K 2003/265 (2013.01); C08L 2201/06 (2013.01);
Abstract

The present invention discloses a biodegradable polyester composition, wherein the biodegradable polyester composition comprises the following components in parts by weight: i) 58 to 80 parts by weight of an aliphatic-aromatic copolyester; ii) 20 to 32 parts by weight of starch; and iii) 0 to 10 parts by weight of a processing agent. The present invention unexpectedly found by research that by using an aliphatic-aromatic copolyester in which an amount of aromatic carboxylic acid accounts for a total amount of diacid is 44 mol % to 48 mol % as a matrix resin, where the aliphatic-aromatic copolyester has a crystallization peak width D of 5° C. to 16° C., and by using starch of which a particle size D (50) is 2 μm to 12 μm as the other phase, and meanwhile by adding a specific amount of a processing agent, the polyester composition prepared has excellent transversal and longitudinal tear strengths, and the polyester composition has a biodegradation rate of 90% or more during the 12-week degradation test, satisfying the industrial compost.