The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 21, 2022

Filed:

Apr. 02, 2018
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Takaaki Tanaka, Tokyo, JP;

Yuki Toji, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); B32B 15/01 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01); C22C 38/38 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B32B 15/013 (2013.01); C21D 6/001 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0236 (2013.01); C22C 38/002 (2013.01); C22C 38/005 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/38 (2013.01); C21D 2211/001 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

A high strength cold rolled steel sheet has a composition which contains, in terms of mass %, more than 0.15% and not more than 0.45% of C, 0.50-2.50% of Si, 1.50-3.00% of Mn, not more than 0.050% of P, not more than 0.0100% of S, 0.010-0.100% of Al and not more than 0.0100% of N, with the remainder including Fe and unavoidable impurities, has a total content of ferrite and bainitic ferrite of 20-80%, has a retained austenite content of more than 10% and not more than 40%, has a martensite content of more than 0% and not more than 50%, and is such that the proportion of retained austenite that has an aspect ratio of not more than 0.5 is not less than 75%, and the proportion of retained austenite having an aspect ratio of not more than 0.5 that is present at Bain group boundaries is not less than 50%.