The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 14, 2022

Filed:

Aug. 17, 2021
Applicant:

Chevron Phillips Chemical Company Lp, The Woodlands, TX (US);

Inventors:

Max P. McDaniel, Bartlesville, OK (US);

Kathy S. Clear, Bartlesville, OK (US);

Jeremy M. Praetorius, Bartlesville, OK (US);

Eric D. Schwerdtfeger, Bartlesville, OK (US);

Mitchell D. Refvik, Kingwood, TX (US);

Mark L. Hlavinka, Kingwood, TX (US);

Assignee:

Chevron Phillips Chemical Company LP, The Woodlands, TX (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 31/02 (2006.01); B01J 31/34 (2006.01); B01J 37/02 (2006.01); B01J 35/10 (2006.01); B01J 21/08 (2006.01); B01J 21/12 (2006.01); B01J 21/06 (2006.01); B01J 31/04 (2006.01);
U.S. Cl.
CPC ...
B01J 31/0209 (2013.01); B01J 21/063 (2013.01); B01J 21/08 (2013.01); B01J 21/12 (2013.01); B01J 31/04 (2013.01); B01J 31/34 (2013.01); B01J 35/1019 (2013.01); B01J 35/1023 (2013.01); B01J 35/1047 (2013.01); B01J 37/024 (2013.01);
Abstract

A method comprising a) contacting a solvent, a carboxylic acid, and a peroxide-containing compound to form an acidic mixture wherein a weight ratio of solvent to carboxylic acid in the acidic mixture is from about 1:1 to about 100:1; b) contacting a titanium-containing compound and the acidic mixture to form a solubilized titanium mixture wherein an equivalent molar ratio of titanium-containing compound to carboxylic acid in the solubilized titanium mixture is from about 1:1 to about 1:4 and an equivalent molar ratio of titanium-containing compound to peroxide-containing compound in the solubilized titanium mixture is from about 1:1 to about 1:20; and c) contacting a chromium-silica support comprising from about 0.1 wt. % to about 20 wt. % water and the solubilized titanium mixture to form an addition product and drying the addition product by heating to a temperature in a range of from about 50° C. to about 150° C. and maintaining the temperature in the range of from about 50° C. to about 150° C. for a time period of from about 30 minutes to about 6 hours to form a pre-catalyst.