The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 24, 2022

Filed:

Sep. 14, 2018
Applicant:

Jsp Corporation, Tokyo, JP;

Inventor:

Tomoo Tokiwa, Kanuma, JP;

Assignee:

JSP CORPORATION, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 5/24 (2006.01); B29B 11/06 (2006.01); B29B 11/16 (2006.01); B29C 44/14 (2006.01); B29C 44/44 (2006.01); B32B 27/20 (2006.01); B32B 27/32 (2006.01); C08J 9/00 (2006.01); C08J 9/228 (2006.01); B29K 23/00 (2006.01); B29K 309/08 (2006.01); B29L 9/00 (2006.01);
U.S. Cl.
CPC ...
B32B 5/245 (2013.01); B29B 11/06 (2013.01); B29B 11/16 (2013.01); B29C 44/14 (2013.01); B29C 44/445 (2013.01); B32B 27/20 (2013.01); B32B 27/32 (2013.01); C08J 9/0085 (2013.01); C08J 9/228 (2013.01); B29K 2023/12 (2013.01); B29K 2309/08 (2013.01); B29L 2009/00 (2013.01); B32B 2262/101 (2013.01); C08J 2323/08 (2013.01); C08J 2323/12 (2013.01); C08J 2323/14 (2013.01);
Abstract

A skin-covered foamed molded article having excellent lightweight property, bending rigidity, and favorable dimensional stability, which includes: a skin material composed of a hollow molded body produced by blow-molding an extruded parison; and an expanded bead molded article located inside the skin material, wherein the skin material has an average wall thickness of from 1.0 mm to 5.0 mm, the skin material includes a glass fiber-reinforced polypropylene-based resin containing glass fiber in a range of from 5 mass % to 30 mass %, the glass fiber has a weight-average fiber length of from 0.4 mm to 1.5 mm, the expanded bead molded article includes a polypropylene-based resin, the peeling strength between the skin material and the expanded bead molded article is 0.1 MPa or higher, and the longitudinal linear expansion coefficient of the skin-covered foamed molded article () at from 23° C. to 80° C. is 7×10−5/° C. or lower.