The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 10, 2022

Filed:

Oct. 10, 2018
Applicant:

Nissan Motor Co., Ltd., Yokohama, JP;

Inventors:

Kenichi Toyoshima, Kanagawa, JP;

Tooru Kosemura, Kanagawa, JP;

Yuichiro Yokoyama, Kyoto, JP;

Yusuke Emori, Kyoto, JP;

Assignee:

NISSAN MOTOR CO., LTD., Yokohama, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/04 (2006.01); H01M 4/36 (2006.01); H01M 4/62 (2006.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
H01M 4/0404 (2013.01); H01M 4/366 (2013.01); H01M 4/624 (2013.01); H01M 10/0525 (2013.01);
Abstract

Provided is a means capable of improving the flatness of a surface of an electrode active material layer in which an electrode active material slurry without assuming addition of a binder. Upon producing a battery electrode which has a current collector and an electrode active material layer disposed on a surface of the current collector and containing an electrode active material, in a coating step of coating an electrode active material slurry in which the electrode active material is dispersed in a solvent on the surface of the current collector to form the electrode active material layer, an electrode active material slurry which has flow characteristics that a region A in which a shear stress is not increased according to an increase in shear rate is present and a region B in which a shear stress is increased and an increase rate thereof is decreased according to an increase in shear rate is present in a region having a shear rate larger than that of the region A, in a shear rate (horizontal axis)-shear stress (vertical axis) curve of the electrode active material slurry, is used as the electrode active material slurry, and, coating of the electrode active material slurry is performed at a coating rate at which the shear rate at the time of coating is a value in which a shear stress equal to or more than a yield stress of the electrode active material slurry is applied in the coating step.