The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 10, 2022

Filed:

Dec. 17, 2018
Applicant:

Stora Enso Oyj, Helsinki, FI;

Inventors:

Kaj Backfolk, Villmanstrand, FI;

Isto Heiskanen, Imatra, FI;

Esa Saukkonen, Lappeenranta, FI;

Katja Lyytikäinen, Imatra, FI;

Assignee:

Stora Enso OYJ, Helsinki, FI;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
D21H 11/18 (2006.01); B32B 27/10 (2006.01); B32B 27/32 (2006.01); D21F 1/00 (2006.01); D21H 17/32 (2006.01); D21H 17/42 (2006.01); D21H 17/45 (2006.01); D21H 21/08 (2006.01); D21H 23/04 (2006.01);
U.S. Cl.
CPC ...
D21H 11/18 (2013.01); B32B 27/10 (2013.01); B32B 27/32 (2013.01); D21F 1/0027 (2013.01); D21H 17/32 (2013.01); D21H 17/42 (2013.01); D21H 17/45 (2013.01); D21H 21/08 (2013.01); D21H 23/04 (2013.01); B32B 2307/72 (2013.01);
Abstract

A method for the production of a fibrous product from a fibrous web, wherein the method comprises the steps of: —providing a fibrous suspension comprising a microfibrillated cellulose, wherein the content of the microfibrillated cellulose of said suspension is in the range of 60 to 99.9 weight-% based on total dry solid content, —adding an uncharged, amphoteric or weakly cationic polymer having a molecular weight of at least 50000 g/mol to said suspension, —adding an anionic polymer having a molecular weight of at least 00000 g/mol to said suspension to provide a mixture of said microfibrillated cellulose, said uncharged, amphoteric or weakly cationic polymer and said anionic polymer, 1—providing said mixture to a substrate to form a fibrous web, wherein the amount of uncharged, amphoteric or weakly cationic polymer in said mixture is in the range of 0.1 to 20 kg/metric ton based on total dry solid content and wherein the amount of anionic polymer in said mixture is in the range of 0.01 to 10 kg/metric ton based on total dry 20 solid content; and—dewatering said fibrous web to form a fibrous product.