The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 10, 2022

Filed:

Mar. 23, 2018
Applicant:

Shin-etsu Chemical Co., Ltd., Tokyo, JP;

Inventors:

Kazuhiro Oishi, Annaka, JP;

Yoshiaki Koike, Annaka, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 183/04 (2006.01); C08K 3/36 (2006.01); C08K 5/14 (2006.01); C08K 3/22 (2006.01); C08K 3/013 (2018.01); C08G 77/18 (2006.01); C08G 77/20 (2006.01); C08G 77/398 (2006.01); C08K 3/38 (2006.01); C08L 83/06 (2006.01); H01B 3/46 (2006.01);
U.S. Cl.
CPC ...
C09J 183/04 (2013.01); C08G 77/18 (2013.01); C08G 77/20 (2013.01); C08G 77/398 (2013.01); C08K 3/013 (2018.01); C08K 3/36 (2013.01); C08K 3/38 (2013.01); C08K 5/14 (2013.01); C08L 83/06 (2013.01); H01B 3/46 (2013.01); C08K 2003/2227 (2013.01); C08K 2003/2296 (2013.01); C08K 2201/001 (2013.01); C08K 2201/005 (2013.01); C08K 2201/006 (2013.01); C08L 2203/202 (2013.01); C08L 2205/03 (2013.01);
Abstract

Provided are a self-welding high dielectric silicone rubber composition and a self-welding high dielectric tape. The self-welding high dielectric silicone rubber composition comprises: (A) 100 parts by mass of an organopolysiloxane represented by an average composition formula (1) and having, in a molecule, at least two alkenyl groups bonded to silicon atoms, RSiO(1), (in the formula, Rrepresents the same or different, unsubstituted or substituted monovalent hydrocarbon group and n is a positive number of 1.95 to 2.04); (B) 10 to 100 parts by mass of hydrophobic fumed silica having a specific surface area obtained by the BET adsorption method of 50 m/g or larger; (C) 100 to 300 parts by mass of a conductive complex oxide; (D) 0.1 to 50 parts by mass of a boric acid or a boric acid compound; (E) 1 to 10 parts by mass of a diorganopolysiloxane capped at both molecular terminals with alkoxy groups; and (F) 0.01 to 10 parts by mass of a curing agent comprising an acyl organic peroxide. The self-welding high dielectric silicone rubber composition can be hot-air vulcanized under normal pressure by extrusion molding or roll forming with calender rolls.