The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 22, 2022

Filed:

Oct. 27, 2017
Applicant:

Corning Incorporated, Corning, NY (US);

Inventors:

Shinu Baby, Painted Post, NY (US);

Dana Craig Bookbinder, Corning, NY (US);

Polly Wanda Chu, Painted Post, NY (US);

Timothy Michael Gross, Corning, NY (US);

Yousef Kayed Qaroush, Painted Post, NY (US);

Assignee:

Corning Incorporated, Corning, NY (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 17/06 (2006.01); B32B 7/12 (2006.01); C03C 17/32 (2006.01); C03C 27/10 (2006.01); B32B 3/08 (2006.01); G06F 1/16 (2006.01); H04M 1/02 (2006.01); G02F 1/1333 (2006.01);
U.S. Cl.
CPC ...
B32B 17/06 (2013.01); B32B 3/08 (2013.01); B32B 7/12 (2013.01); C03C 17/32 (2013.01); C03C 27/10 (2013.01); B32B 2255/26 (2013.01); B32B 2307/546 (2013.01); B32B 2307/581 (2013.01); B32B 2315/08 (2013.01); B32B 2379/08 (2013.01); B32B 2457/20 (2013.01); G02F 1/133305 (2013.01); G06F 1/1652 (2013.01); H04M 1/0268 (2013.01);
Abstract

A glass article having a first glass layer, a second glass layer disposed adjacent to the first glass layer, and an interface slidably coupling the first glass layer to the second glass layer. The interface has a thickness of from 2 nm to 500 nm. The glass article is characterized by: (a) an absence of failure when the article is held at a parallel plate separation distance of 10 mm for 60 minutes at 25° C. and 50% relative humidity; (b) a puncture resistance of greater than about 6 kgf when the second glass layer is supported by (i) a 50 μm thick pressure-sensitive adhesive having an elastic modulus of less than 1 GPa and (ii) an approximately 100 μm thick polyethylene terephthalate layer having an elastic modulus of less than 10 GPa, and the first glass layer is loaded with a tungsten carbide ball having a 1 mm diameter.