The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 01, 2022

Filed:

Apr. 30, 2021
Applicant:

Contemporary Amperex Technology Co., Limited, Ningde, CN;

Inventors:

Zhijie Gong, Ningde, CN;

Bin Xie, Ningde, CN;

Shitong Chen, Ningde, CN;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 24/00 (2006.01); C21D 8/02 (2006.01); H01M 4/36 (2006.01); H01M 4/38 (2006.01); H01M 10/0525 (2010.01); H01M 4/04 (2006.01); H01M 4/40 (2006.01); B21B 1/40 (2006.01);
U.S. Cl.
CPC ...
C22C 24/00 (2013.01); C21D 8/0236 (2013.01); H01M 4/0435 (2013.01); H01M 4/366 (2013.01); H01M 4/382 (2013.01); H01M 10/0525 (2013.01); B21B 1/40 (2013.01); H01M 4/405 (2013.01);
Abstract

The present embodiments provide a metal lithium strip, a prelithiated electrode plate, and a prelithiation process. The metal lithium strip comprises a lithium substrate and a metal element doped in the lithium substrate, the metal element comprises at least two of magnesium, boron, aluminum, silicon, indium, zinc, silver, calcium, manganese and sodium; and the metal lithium strip has a strength a, a width w, and a thickness h, satisfying: σ-(w/105h)>0. In the present application, the strength of the lithium strip is adjusted by the doping of the metal elements; meanwhile, the strength of the adjusted lithium strip is matched with its width and thickness ensuring that in the process of rolling the metal lithium strip to a reasonable thickness, the phenomenon of edge cracking of the lithium strip is avoided, lithium metal resources and production costs can be saved, a uniform pre-lithiation effect for electrode plate can also be achieved.


Find Patent Forward Citations