The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 22, 2022

Filed:

Jul. 13, 2018
Applicant:

Lg Chem, Ltd., Seoul, KR;

Inventors:

Sang Soon Choi, Daejeon, KR;

Seung Beom Cho, Daejeon, KR;

Hyun Ah Park, Daejeon, KR;

Won Sig Jung, Daejeon, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); C01G 53/00 (2006.01); H01M 4/505 (2010.01); H01M 10/0525 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); C01G 53/50 (2013.01); H01M 4/505 (2013.01); H01M 10/0525 (2013.01); C01P 2002/52 (2013.01); C01P 2006/40 (2013.01); H01M 2004/028 (2013.01);
Abstract

A method of preparing a positive electrode active material which includes forming a pre-sintered mixture by adding a reaction mixture including a lithium raw material and a nickel-manganese-cobalt precursor to a first crucible and performing a primary heat treatment at a temperature of 500° C. to 800° C., and, after discharging the pre-sintered mixture from the first crucible, adding the pre-sintered mixture to a second crucible and performing a secondary heat treatment at a temperature of 700° C. to 1,000° C. to form a lithium nickel manganese cobalt-based positive electrode active material, wherein a volume of the pre-sintered mixture formed after the primary heat treatment is 20% to 50% of a volume of the reaction mixture added to the first crucible.